Why temperature matters even when measuring cold
At 40 °C the aluminium beam and steel rail expand differently, so 7 μm cold may become 9 or 5 μm hot, possibly reversing sign.
The report must state the measurement temperature and an estimated hot correction. '7 μm' without conditions gives the process nothing.
Shape of the undulation
Accumulated height rises to +4.2 μm, falls to −5.5 μm and returns to −0.5 μm: a classic mid-span sag. Peak-to-valley against a fitted line is 7.0 μm.
That shape points to mid-span support stiffness rather than rail straightness. A bent rail would show shorter-period waviness, not one bow.
Fix and verification
Add mid-span support or increase beam section stiffness first; shimming only changes end heights and cannot remove sag.
Re-measure with the same span and direction, then again hot. Only when both are within 5 μm is it resolved.
Case workflow, animated
- Confirm the task and datum
- Lay out stations by span
- Acquire readings and convert
- Evaluate and verify
The animation follows the station layout and calculation order of this case. Values are teaching data.
Teaching data. Real layer uniformity also depends on roller or blade condition, powder flow and build-plate flatness; gantry straightness is one input only.